2.0853 (CuNi1,5Si)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | 2.0800-2.0899 |
Chemical composition
| Standard | Si, % | Cu, % | Ni, % | ET, % |
|---|---|---|---|---|
| DIN 17666 | 0.4–0.7 | 97.2–98.6 | 1–1.6 | < 0.5 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| DIN 17666 | |
| DIN 17672 Part 1 | |
| DIN 17672 Part 2 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| ET | % | Total other items |
| Si | % | Silicon |
| Cu | % | Copper |
| Ni | % | Nickel |