2.0855 (CuNi2si)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | 2.0800-2.0899 |
Chemical composition
| Standard | Si, % | Mn, % | Cu, % | Ni, % | ET, % |
|---|---|---|---|---|---|
| DIN 17666 | 0.5–0.8 | < 0.8 | 95.4–97.9 | 1.6–2.5 | < 0.5 |
Information on suppliers
Analogues
| USA | CIS, Russia, Ukraine |
|---|---|
| C64700 | CuNi2Si |
Standards
| Standard | Description |
|---|---|
| DIN 17666 | |
| DIN 17672 Part 1 | |
| DIN 17672 Part 2 | |
| DIN 17673 Part 1 | |
| DIN 17673 Part 2 | |
| DIN 17678 Part 2 | |
| DIN 17678 Part 1 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| ET | % | Total other items |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cu | % | Copper |
| Ni | % | Nickel |