2.0875 (CuNi9Sn2)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | 2.0800-2.0899 |
Chemical composition
| Standard | Fe, % | Sn, % | Mn, % | Co, % | Cu, % | Zn, % | Ni, % | Pb, % | ET, % |
|---|---|---|---|---|---|---|---|---|---|
| DIN 17664 | < 0.3 | 1.8–2.8 | < 0.3 | < 0.5 | 85.37–89.7 | < 0.1 | 8.5–10.5 | < 0.03 | < 0.1 |
Note: Ni: Ni + Co
Information on suppliers
Analogues
| USA |
|---|
| C72500 |
Standards
| Standard | Description |
|---|---|
| DIN 17664 | |
| DIN 17670 Part 1 | |
| DIN 17670 Part 2 | |
| DIN 1777 | |
| DIN 1780 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| ET | % | Total other items |
| Fe | % | Iron |
| Sn | % | Tin |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Pb | % | Lead |