2.0921 (CuAl7)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | 2.0900-2.0999 |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cu, % | Zn, % | Ni, % | Al, % | Pb, % | Примеси, % |
|---|---|---|---|---|---|---|---|---|---|
| DIN 1733 Part 1 | < 0.5 | < 0.2 | < 1 | 87.38–92.5 | < 0.2 | < 0.8 | 7.5–9.5 | < 0.02 | < 0.4 |
Information on suppliers
Analogues
| USA |
|---|
| C61000 |
Standards
| Standard | Description |
|---|---|
| DIN 1733 Part 1 | |
| DIN 8566 Part 1 |