2.093 (EL-CuAl9Ni2Fe)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | 2.0900-2.0999 |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cu, % | Ni, % | Al, % | Pb, % | Примеси, % |
|---|---|---|---|---|---|---|---|---|
| DIN 1733 Part 1 | 1.5–2.5 | < 0.7 | 1.5–3 | 81.78–88.7 | 1.8–3 | 6.5–8.5 | < 0.02 | < 0.5 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| DIN 1733 Part 1 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cu | % | Copper |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Pb | % | Lead |