2.0936 (CuAl10Fe3Mn2)
Classification
| Country |
Section |
Category |
| Germany |
Alloy DIN 17007−4 |
2.0900-2.0999 |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cu, % |
Zn, % |
Ni, % |
Al, % |
Pb, % |
ET, % |
| DIN 17665 |
2–4 |
< 0.2 |
1.5–3.5 |
79.45–88 |
< 0.5 |
< 1 |
8.5–11 |
< 0.05 |
< 0.3 |
Information on suppliers
Analogues
| CIS, Russia, Ukraine |
| Бр.ВАЖМц |
| C63280 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| ET |
% |
Total other items |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| Pb |
% |
Lead |