2.0941 (FeAlBz)
Classification
| Country |
Section |
Category |
| Germany |
Alloy DIN 17007−4 |
2.0900-2.0999 |
Chemical composition
| Standard |
Fe, % |
Si, % |
Sn, % |
Mg, % |
Mn, % |
Cu, % |
Zn, % |
Ni, % |
Al, % |
Pb, % |
Примеси, % |
| DIN 17656 |
2–3.8 |
0.1–0.2 |
< 0.2 |
< 0.04 |
0.8–1 |
83–89 |
< 0.4 |
< 2.7 |
8.7–10.7 |
0.1–0.2 |
< 0.7 |
Information on suppliers
Analogues
| USA |
CIS, Russia, Ukraine |
| C63280 |
CuAl10Fe3Mn2 |