2.096
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | 2.0900-2.0999 |
Chemical composition
| Standard | Fe, % | Mn, % | Cu, % | Zn, % | Ni, % | Al, % | Pb, % | ET, % |
|---|---|---|---|---|---|---|---|---|
| DIN 17665 | < 1.5 | 1.5–3 | 83.85–90.5 | < 0.5 | < 0.8 | 8–10 | < 0.05 | < 0.3 |
Information on suppliers
Analogues
| USA | CIS, Russia, Ukraine |
|---|---|
| C61810 | БрАМц9-2 |
Standards
| Standard | Description |
|---|---|
| DIN 17665 | |
| DIN 17672 Part 1 | |
| DIN 17672 Part 2 | |
| DIN 8566 Part 2 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| ET | % | Total other items |
| Fe | % | Iron |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Pb | % | Lead |