2.0966 (CuAl10Ni5Fe4)
Classification
| Country |
Section |
Category |
| Germany |
Alloy DIN 17007−4 |
2.0900-2.0999 |
Chemical composition
| Standard |
Fe, % |
Mn, % |
Cu, % |
Zn, % |
Ni, % |
Al, % |
Pb, % |
Pd, % |
Примеси, % |
| DIN 17665 |
2.5–5.3 |
< 1.5 |
75.2–85 |
< 0.5 |
4–6 |
8.5–11 |
< 0.05 |
< 0.15 |
< 0.3 |