Chemical composition
| Standard |
Fe, % |
Si, % |
Sn, % |
Mg, % |
Mn, % |
Cu, % |
Zn, % |
Ni, % |
Al, % |
Pb, % |
Примеси, % |
| DIN 1714 |
3.5–5.5 |
< 0.1 |
< 0.2 |
< 0.05 |
< 3 |
> 76 |
< 0.5 |
4–6.5 |
8.5–11 |
< 0.05 |
< 0.8 |