2.1006
Classification
| Country |
Section |
Category |
| Germany |
Alloy DIN 17007−4 |
2.1000-2.1099 |
Chemical composition
| Standard |
Fe, % |
Si, % |
Sn, % |
Bi, % |
Mn, % |
Cu, % |
Ni, % |
Sb, % |
Al, % |
Te, % |
Pb, % |
As, % |
P, % |
Примеси, % |
| DIN 1733 Part 1 |
< 0.05 |
0.1–0.5 |
0.4–1 |
< 0.002 |
0.1–0.5 |
> 98 |
< 0.3 |
< 0.005 |
< 0.01 |
< 0.001 |
< 0.01 |
< 0.05 |
< 0.02 |
< 0.1 |