2.1016
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | 2.1000-2.1099 |
Chemical composition
| Standard | Fe, % | Sn, % | Cu, % | Zn, % | Ni, % | Pb, % | P, % | ET, % |
|---|---|---|---|---|---|---|---|---|
| DIN 17662 | < 0.1 | 3.5–4.5 | 94.2–96.49 | < 0.3 | < 0.3 | < 0.05 | 0.01–0.35 | < 0.2 |
Information on suppliers
Analogues
| CIS, Russia, Ukraine | USA |
|---|---|
| БОФ4 | C51180 |
Standards
| Standard | Description |
|---|---|
| DIN 17670 Part 1 | |
| DIN 17670 Part 2 | |
| DIN 1777 | |
| DIN 1780 | |
| DIN 17662 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| ET | % | Total other items |
| Fe | % | Iron |
| Sn | % | Tin |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Pb | % | Lead |
| P | % | Phosphorus |