2.1022
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | 2.1000-2.1099 |
Chemical composition
| Standard | Fe, % | Sn, % | Cu, % | Zn, % | Al, % | Pb, % | P, % | Примеси, % |
|---|---|---|---|---|---|---|---|---|
| DIN 1733 Part 1 | < 0.1 | 5–8 | 90.97–94.99 | < 0.1 | < 0.01 | < 0.02 | 0.01–0.4 | < 0.4 |
Note: DIN 1733 T.1: P 0.01-0.35
Information on suppliers
Analogues
| CIS, Russia, Ukraine |
|---|
| C51800 |
Standards
| Standard | Description |
|---|---|
| DIN 1733 Part 1 | |
| DIN 8566 Part 1 | |
| DIN 8566 Part 2 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Sn | % | Tin |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |
| Pb | % | Lead |
| P | % | Phosphorus |