2.1057 (CuSn14)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | 2.1000-2.1099 |
Chemical composition
| Standard | Si, % | Sn, % | Cu, % | Ni, % | Al, % | Pb, % |
|---|---|---|---|---|---|---|
| DIN 17656 | < 0.01 | 13.3–15 | 85–86.5 | < 0.8 | < 0.01 | < 0.8 |
Information on suppliers
Analogues
| USA |
|---|
| C90800 |
Standards
| Standard | Description |
|---|---|
| DIN 17656 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Si | % | Silicon |
| Sn | % | Tin |
| Cu | % | Copper |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Pb | % | Lead |