2.1176 (CuPb10Sn)
Classification
| Country |
Section |
Category |
| Germany |
Alloy DIN 17007−4 |
2.1100-2.1199 |
Chemical composition
| Standard |
Fe, % |
Sn, % |
Cu, % |
Zn, % |
Ni, % |
Sb, % |
Pb, % |
P, % |
Примеси, % |
| DIN 1716 |
< 0.25 |
9–11 |
78–82 |
< 2 |
< 1.5 |
< 0.5 |
8–11 |
< 0.05 |
< 0.5 |
Information on suppliers
Analogues
| USA |
CIS, Russia, Ukraine |
| C93700 |
БрО10Ф1 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Примеси |
% |
Impurities |
| Sn |
% |
Tin |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Sb |
% |
Antimony |
| Pb |
% |
Lead |
| P |
% |
Phosphorus |