2.1183 (Snpbbz)
Classification
| Country |
Section |
Category |
| Germany |
Alloy DIN 17007−4 |
2.1100-2.1199 |
Chemical composition
| Standard |
Fe, % |
Si, % |
Sn, % |
Mn, % |
Cu, % |
Zn, % |
Ni, % |
Sb, % |
Al, % |
Pb, % |
As, % |
P, % |
S, % |
Примеси, % |
| DIN 17656 |
< 0.15 |
< 0.01 |
7.3–9 |
< 0.1 |
75–78.5 |
< 2 |
< 1.8 |
< 0.4 |
< 0.01 |
13.5–16.5 |
< 0.1 |
< 0.03 |
< 0.08 |
< 0.4 |
Information on suppliers
Analogues
| USA |
CIS, Russia, Ukraine |
| C93800 |
78-7-15 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Примеси |
% |
Impurities |
| Si |
% |
Silicon |
| Sn |
% |
Tin |
| Mn |
% |
Manganese |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Sb |
% |
Antimony |
| Al |
% |
Aluminium |
| Pb |
% |
Lead |
| As |
% |
Arsenic |
| P |
% |
Phosphorus |
| S |
% |
Sulfur |