2.4068 (LC-Ni99)
Classification
| Country |
Section |
Category |
| Germany |
Alloy DIN 17007−4 |
Pure Nickel and Cobalt |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mg, % |
Mn, % |
Co, % |
Ti, % |
Cu, % |
Ni, % |
C, % |
S, % |
| DIN 17740 |
< 0.4 |
< 0.25 |
< 0.15 |
< 0.35 |
< 1 |
< 0.1 |
< 0.25 |
< 99 |
< 0.02 |
< 0.005 |