2.4106 (NiMn1)
Classification
| Country |
Section |
Category |
| Germany |
Alloy DIN 17007−4 |
Ni and Co Low Alloyed Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mg, % |
Mn, % |
Co, % |
Ti, % |
Cu, % |
Ni, % |
C, % |
S, % |
| DIN 17741 |
< 0.5 |
< 0.25 |
< 0.15 |
0.4–1 |
< 1 |
< 0.1 |
< 0.5 |
< 98 |
< 0.15 |
< 0.01 |