2.4128
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | Ni and Co Low Alloyed Alloys |
Chemical composition
| Standard | Ti, % | Ni, % | Al, % |
|---|---|---|---|
| 0.5 | 95 | 4.5 |
Information on suppliers
Analogues
| USA |
|---|
| N03301 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Ti | % | Titan |
| Ni | % | Nickel |
| Al | % | Aluminium |