2.4508
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | Ni-Fe and Co-Fe Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Cu, % | Ni, % | C, % |
|---|---|---|---|---|---|---|---|
| 15–18 | < 0.3 | < 1 | 1.5–2.5 | 4–6 | 72.15–79.5 | < 0.05 |
Information on suppliers
Analogues
| CIS, Russia, Ukraine |
|---|
| ЭП254 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| C | % | Carbon |