2.4603 (NICr30FeMo)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | Ni Alloys with Co, Cr and Mo Co Alloys with Cr, Ni and Mo |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Co, % | Cr, % | Cu, % | Ni, % | P, % | C, % | S, % | Nb, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 13–17 | < 0.08 | < 2 | < 5 | 28–31.5 | 1–2.4 | 30.43–52.2 | < 0.04 | < 0.03 | < 0.02 | 0.3–1.5 | 4–6 | 1.5–4 |
Information on suppliers
Analogues
| USA | CIS, Russia, Ukraine |
|---|---|
| N06002 | NiCr22Fe18Mo |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Nb | % | Niobium |
| Mo | % | Molybdenum |
| W | % | Tungsten |