2.461 (NiMo16Cr16Ti)
Classification
| Country |
Section |
Category |
| Germany |
Alloy DIN 17007−4 |
Ni Alloys with Co, Cr and Mo Co Alloys with Cr, Ni and Mo |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Co, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
| DIN 17744 |
< 3 |
< 0.08 |
< 1 |
< 2 |
14–18 |
< 0.7 |
< 0.5 |
57.665–72 |
< 0.025 |
< 0.015 |
< 0.015 |
14–17 |
Information on suppliers
Analogues
| USA |
CIS, Russia, Ukraine |
| N06455 |
NiCr16Mo15Ti |
Standards