2.4623 (EL-NiCr23Mo7Cu)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | Ni Alloys with Co, Cr and Mo Co Alloys with Cr, Ni and Mo |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Co, % | Cr, % | Cu, % | Ni, % | Zr, % | P, % | C, % | S, % | Mo, % | W, % | Ta, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 18–21 | < 1 | < 1 | < 5 | 21–23.5 | 1.5–2.5 | 35.81–53.49 | 0.01–0.1 | < 0.04 | < 0.02 | < 0.03 | 6–8 | < 1.5 | < 0.5 |
Information on suppliers
Analogues
| USA | CIS, Russia, Ukraine |
|---|---|
| W86985 | NiCr22Mo7Fe19 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| Zr | % | Zirconium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| W | % | Tungsten |
| Ta | % | Tantalum |