2.4641 (NiCr21Mo6Cu)
Classification
| Country |
Section |
Category |
| Germany |
Alloy DIN 17007−4 |
Ni Alloys with Co, Cr and Mo Co Alloys with Cr, Ni and Mo |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Co, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
Al, % |
P, % |
C, % |
S, % |
Mo, % |
| DIN 17744 |
17.235–33.4 |
< 0.5 |
< 1 |
< 1 |
20–23 |
0.6–1 |
1.5–3 |
29.835–55.165 |
< 0.2 |
< 0.025 |
< 0.025 |
< 0.015 |
5.5–7 |
Information on suppliers
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Co |
% |
Cobalt |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |