2.4647 (NiCr25FeAIYC)
Classification
| Country |
Section |
Category |
| Germany |
Alloy DIN 17007−4 |
Ni Alloys with Co, Cr and Mo Co Alloys with Cr, Ni and Mo |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
Zr, % |
Al, % |
P, % |
C, % |
S, % |
Y, % |
| DIN 17742 |
8–11 |
< 0.5 |
< 0.1 |
24–26 |
0.1–0.25 |
< 0.15 |
58.315–65.24 |
0.01–0.1 |
2.4–3 |
< 0.02 |
0.2–0.4 |
< 0.015 |
0.05–0.15 |
Information on suppliers
Analogues
| CIS, Russia, Ukraine |
| NiCr25Fe10Al3YC |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| Zr |
% |
Zirconium |
| Al |
% |
Aluminium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Y |
% |
Yttrium |