2.4657 (EL-NiCr19Mo15)
Classification
| Country |
Section |
Category |
| Germany |
Alloy DIN 17007−4 |
Ni Alloys with Co, Cr and Mo Co Alloys with Cr, Ni and Mo |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
V, % |
C, % |
S, % |
Nb, % |
Mo, % |
| DIN 1736 Part 1 |
< 1.5 |
< 0.4 |
< 2 |
18–20 |
59.26–68 |
< 0.4 |
< 0.025 |
< 0.015 |
< 0.4 |
14–16 |