2.4671 (G-NiCr12Al6MoNb)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | Ni Alloys with Co, Cr and Mo Co Alloys with Cr, Ni and Mo |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | Zr, % | Al, % | P, % | C, % | S, % | Nb, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| < 2.5 | < 0.5 | 0.005–0.015 | < 0.25 | < 1 | 12–14 | 0.5–1 | < 0.5 | 65.355–76.31 | 0.005–0.15 | 5.5–6.5 | < 0.015 | 0.08–0.2 | < 0.015 | 1.8–2.8 | 3.8–5.2 |