2.4698 (SG-NiCr23Mo16Cu)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | Ni Alloys with Co, Cr and Mo Co Alloys with Cr, Ni and Mo |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Co, % | Cr, % | Cu, % | Ni, % | Al, % | P, % | C, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| < 3 | < 0.08 | < 0.5 | < 2 | 22–24 | 1.3–1.9 | 50.985–61.7 | < 0.5 | < 0.025 | < 0.01 | 15–17 |
Information on suppliers
Analogues
| USA | CIS, Russia, Ukraine |
|---|---|
| W86200 | NiCr23Mo16Cu2 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| Mo | % | Molybdenum |