2.4831 (SG (UP) -NiCr21Mo9Nb)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | Ni Alloys with Co, Cr and Mo Co Alloys with Cr, Ni and Mo |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | Al, % | C, % | S, % | Nb, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| < 5 | < 0.5 | < 0.5 | < 1 | 20–23 | < 0.4 | < 0.5 | < 60 | < 0.4 | < 0.1 | < 0.015 | 3–4.5 | 8–10 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| Al | % | Aluminium |
| C | % | Carbon |
| S | % | Sulfur |
| Nb | % | Niobium |
| Mo | % | Molybdenum |