3.0205 (Al99.0)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-ferrous metals | Pure aluminium |
Chemical composition
| Standard | Fe, % | Mg, % | Mn, % | Ti, % | Cu, % | Zn, % | OE, % | ET, % |
|---|---|---|---|---|---|---|---|---|
| DIN 1712 Part 3 | < 1 | < 0.05 | < 0.05 | < 0.05 | < 0.05 | < 0.1 | < 0.15 | < 1 |
Note: Si+Fe < 1.0
Information on suppliers
Analogues
| Russia | USA |
|---|---|
| АДС | 1200 AA |
Standards
| Standard | Description |
|---|---|
| DIN 1712 Part 3 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| ET | % | Total other items |
| Fe | % | Iron |
| OE | % | Other items |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |