3.0256 (E-AlH)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-ferrous metals | Pure aluminium |
Chemical composition
| Standard | Fe, % | Si, % | Cu, % | Zn, % | Al, % | Примеси, % | OE, % |
|---|---|---|---|---|---|---|---|
| DIN 1712 Part 1 | < 0.35 | < 0.2 | < 0.02 | < 0.04 | > 98.86 | < 0.5 | < 0.03 |
Note: Cr + Mn + Ti + V < 0.03
Information on suppliers
Analogues
| Russia | USA |
|---|---|
| АД0 | 150.1 ANSI |
Standards
| Standard | Description |
|---|---|
| DIN 1712 Part 1 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| OE | % | Other items |
| Примеси | % | Impurities |
| Si | % | Silicon |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |