3.028 (Al99,8H)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-ferrous metals | Pure aluminium |
Chemical composition
| Standard | Fe, % | Si, % | Ti, % | Cu, % | Zn, % | Al, % | Примеси, % | OE, % |
|---|---|---|---|---|---|---|---|---|
| DIN 1712 Part 1 | < 0.15 | < 0.15 | < 0.02 | < 0.01 | < 0.04 | > 99.63 | < 0.2 | < 0.02 |
Information on suppliers
Analogues
| Russia | USA |
|---|---|
| А8 | 1080A |