3.0881 (V-AlTi10)
Classification
| Country |
Section |
Category |
| Germany |
Non-ferrous metals |
Al alloys with: Ti, B, be, Zr |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mg, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
V, % |
Al, % |
Примеси, % |
OE, % |
| DIN 1725 Part 3 |
< 0.3 |
< 0.2 |
< 0.02 |
< 0.02 |
< 0.02 |
9–11 |
< 0.02 |
< 0.04 |
< 0.3 |
88.08–91 |
< 0.15 |
< 0.05 |