3.2166 (GBD-AlSi9Cu3)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-ferrous metals | AlSi alloys with: Cu |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mg, % | Mn, % | Ti, % | Cu, % | Zn, % | Ni, % | Al, % | Pb, % | OE, % | ET, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| DIN 1725 Part 5 | < 1 | 8–11 | < 0.1 | 0.1–0.5 | 0.1–0.4 | < 0.15 | 2–3.5 | < 1.2 | < 0.3 | 81.65–89.8 | < 0.2 | < 0.05 | < 0.15 |
Note: По договоренности : Fe < 0.80%
Information on suppliers
Analogues
| Russia | USA |
|---|---|
| В2616 | SC 84B |
Standards
| Standard | Description |
|---|---|
| DIN 1725 Part 5 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| ET | % | Total other items |
| Fe | % | Iron |
| OE | % | Other items |
| Si | % | Silicon |
| Sn | % | Tin |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Pb | % | Lead |