3.2305 (Alldrey)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-ferrous metals | AlSi alloys with: Mg |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Cu, % | Zn, % | Al, % | OE, % | ET, % |
|---|---|---|---|---|---|---|---|---|
| DIN 1725 Part 1 | 0.1–0.3 | 0.5–0.6 | 0.35–0.6 | < 0.02 | < 0.15 | 98.33–99.05 | < 0.05 | < 0.15 |
Note: Cr + Mn + Ti + V < 0.03
Information on suppliers
Analogues
| Russia | USA |
|---|---|
| АД31 | 6101A AA |
Standards
| Standard | Description |
|---|---|
| DIN 1725 Part 1 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| ET | % | Total other items |
| Fe | % | Iron |
| OE | % | Other items |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |