3.2332 (GB-AlSi10Mg(Cu))
Classification
| Country |
Section |
Category |
| Germany |
Non-ferrous metals |
AlSi alloys with: Mg |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mg, % |
Mn, % |
Ti, % |
Cu, % |
Zn, % |
Ni, % |
Al, % |
OE, % |
ET, % |
| DIN 1725 Part 5 |
< 0.6 |
9–11 |
0.2–0.5 |
0.1–0.4 |
< 0.15 |
< 0.3 |
< 0.3 |
< 0.1 |
86.65–90.7 |
< 0.05 |
< 0.15 |
Information on suppliers
Analogues
| Russia |
USA |
| АК9пч |
EN AC-43000 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| ET |
% |
Total other items |
| Fe |
% |
Iron |
| OE |
% |
Other items |
| Si |
% |
Silicon |
| Mg |
% |
Magnesium |
| Mn |
% |
Manganese |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |