3.2384
Aerospace Series — 7Si-0.6Mg Deformable Aluminum Alloy — Part 5: Weld metal for welding.
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-ferrous metals | AlSi alloys with: Mg |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Ti, % | Cu, % | Zn, % | Al, % | OE, % | ET, % |
|---|---|---|---|---|---|---|---|---|---|---|
| DIN WL 3.2384-5-2012 | < 0.2 | 6.5–7.5 | 0.5–0.8 | < 0.1 | < 0.2 | < 0.05 | < 0.1 | 91.05–93 | < 0.05 | < 0.15 |
Note: Due to burnout during welding, the Mn content is higher than that of the cast alloy
Information on suppliers
Standards
| Standard | Description |
|---|---|
| DIN WL 3.2384-5-2012 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| ET | % | Total other items |
| Fe | % | Iron |
| OE | % | Other items |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |