3.3207 (E-AlMgSi0.5)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-ferrous metals | AlMg alloys with: Si |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Cu, % | Zn, % | Al, % | OE, % | ET, % |
|---|---|---|---|---|---|---|---|---|---|
| DIN 1725 Part 1 | 0.1–0.3 | 0.3–0.6 | 0.35–0.6 | < 0.05 | < 0.05 | < 0.1 | 98.3–99.25 | < 0.03 | < 0.1 |
Note: Cr + Mn + Ti + V < 0.03
Information on suppliers
Analogues
| Russia | USA |
|---|---|
| АД31 | 6101A AA |
Standards
| Standard | Description |
|---|---|
| DIN 1725 Part 1 |