3.321 (AlMgSi0.7)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-ferrous metals | AlMg alloys with: Si |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Cr, % | Ti, % | Cu, % | Zn, % | Ni, % | Al, % | OE, % | ET, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| DIN 1725 Part 1 | < 0.35 | 0.5–0.9 | 0.4–0.7 | < 0.5 | < 0.3 | < 0.1 | < 0.3 | < 0.2 | < 0.1 | 96.55–99.1 | < 0.05 | < 0.15 |
Note: Cr + Mn 0.12 - 0.50%
Information on suppliers
Analogues
| Russia | USA |
|---|---|
| АД31 | 6005B AA |
Standards
| Standard | Description |
|---|---|
| DIN 1725 Part 1 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| ET | % | Total other items |
| Fe | % | Iron |
| OE | % | Other items |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |