3.3262 (GB-AlMg5Si)
Classification
| Country |
Section |
Category |
| Germany |
Non-ferrous metals |
AlMg alloys with: Si |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mg, % |
Mn, % |
Ti, % |
Cu, % |
Zn, % |
Al, % |
OE, % |
ET, % |
| DIN 1725 Part 5 |
< 0.4 |
0.9–1.5 |
4.8–5.5 |
0.001–0.4 |
0.001–0.2 |
< 0.03 |
< 0.1 |
91.87–94.298 |
< 0.05 |
< 0.15 |
Information on suppliers
Analogues
| Russia |
USA |
| АМг4К1,5М |
EN AC-51400 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| ET |
% |
Total other items |
| Fe |
% |
Iron |
| OE |
% |
Other items |
| Si |
% |
Silicon |
| Mg |
% |
Magnesium |
| Mn |
% |
Manganese |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Al |
% |
Aluminium |