3.3309 (AlRMg0.5)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-ferrous metals | AlMg binary alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Ti, % | Zn, % | Al, % | Примеси, % | OE, % |
|---|---|---|---|---|---|---|---|---|
| DIN 1725 Part 1 | < 0.008 | < 0.01 | 0.35–0.6 | < 0.008 | < 0.01 | 99.364–99.65 | < 0.02 | < 0.003 |
Note: Fe + Ti < 0.008