3.3354 (AlMg5)
Aerospace Series — 5Mg Deformable Aluminum Alloy — Part 1: Rivets and Rivet Wire
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-ferrous metals | AlMg binary alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Cr, % | Cu, % | Zn, % | Al, % | OE, % | ET, % |
|---|---|---|---|---|---|---|---|---|---|---|
| DIN WL 3.3354-1-2012 | < 0.5 | < 0.4 | 4.5–5.6 | 0.1–0.6 | < 0.2 | < 0.1 | < 0.2 | 92.4–95.4 | < 0.05 | < 0.15 |
Note: Ti + Zr < 0.20 Mn + Cr : 0.10 - 0.60
Information on suppliers
Analogues
| Russia | USA |
|---|---|
| АМг5 | 5019 AA |
Standards
| Standard | Description |
|---|---|
| DIN WL 3.3354-1-2012 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| ET | % | Total other items |
| Fe | % | Iron |
| OE | % | Other items |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |