3.3535 (AlMg3)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-ferrous metals | AlMg alloys with: Mn, Cr |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Ti, % | Cu, % | Zn, % | Al, % | OE, % | ET, % |
|---|---|---|---|---|---|---|---|---|---|---|
| DIN 1725 Part 1 | < 0.4 | < 0.4 | 2.6–3.6 | < 0.5 | < 0.15 | < 0.1 | < 0.2 | 94.65–97.4 | < 0.05 | < 0.15 |
Note: Cr + Mn 0.10 - 0.60%
Information on suppliers
Analogues
| Russia | USA |
|---|---|
| АМг3С | 5754 AA |
Standards
| Standard | Description |
|---|---|
| DIN 1725 Part 1 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| ET | % | Total other items |
| Fe | % | Iron |
| OE | % | Other items |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |