3.3536 (SG-AlMg3)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-ferrous metals | AlMg alloys with: Mn, Cr |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Cr, % | Ti, % | Cu, % | Zn, % | Al, % | Примеси, % | OE, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| DIN 1732 Part 1 | < 0.4 | < 0.25 | 2.6–3.6 | 0.1–0.6 | < 0.3 | < 0.15 | < 0.05 | < 0.2 | 94.45–97.3 | < 0.15 | < 0.05 |
Note: Mn + Cr: 0.10 - 0.60 Cr > 0.10% or Mn > 0.20%
Information on suppliers
Analogues
| Russia | USA |
|---|---|
| АМг3С | 5754 AA |
Standards
| Standard | Description |
|---|---|
| DIN 1732 Part 1 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| OE | % | Other items |
| Примеси | % | Impurities |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |