3.4335 (AlZnMg1)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-ferrous metals | AlZn alloys with: Mg |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Cr, % | Cu, % | Zn, % | Zr, % | Al, % | OE, % | ET, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| DIN 1725 | < 0.4 | < 0.35 | 1–1.4 | 0.05–0.5 | 0.1–0.35 | < 0.2 | 4–5 | 0.08–0.2 | 91.6–94.77 | < 0.05 | < 0.15 |
Note: Ti + Zr: 0.08 - 0.25
Information on suppliers
Analogues
| Russia | USA |
|---|---|
| 1915 | 7005 AA |
Standards
| Standard | Description |
|---|---|
| DIN 1725 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| ET | % | Total other items |
| Fe | % | Iron |
| OE | % | Other items |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Cu | % | Copper |
| Zn | % | Zinc |
| Zr | % | Zirconium |
| Al | % | Aluminium |