3.4337 (Al99.8ZnMg)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-ferrous metals | AlZn alloys with: Mg |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Cr, % | Ti, % | Cu, % | Zn, % | Zr, % | Al, % | OE, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| DIN 1725 Part 1 | < 0.1 | < 0.1 | 0.7–1.2 | < 0.05 | < 0.1 | < 0.02 | < 0.2 | 3.8–4.6 | < 0.15 | 93.48–95.5 | < 0.02 |
Note: Fe + Si + Mn < 0.20
Information on suppliers
Standards
| Standard | Description |
|---|---|
| DIN 1725 Part 1 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| OE | % | Other items |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Zr | % | Zirconium |
| Al | % | Aluminium |