3.4394
Classification
| Country |
Section |
Category |
| Germany |
Non-ferrous metals |
AlZn alloys with: Mg |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mg, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Zn, % |
Ni, % |
Zr, % |
Al, % |
OE, % |
ET, % |
| DIN WL 3.4394-2-2012 |
< 0.15 |
< 0.12 |
2.1–2.6 |
< 0.1 |
< 0.05 |
< 0.06 |
1.5–2 |
5.7–6.7 |
< 0.05 |
0.1–0.16 |
88.01–90.6 |
< 0.05 |
< 0.15 |