3.4415 (AlZn1)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-ferrous metals | AAlZn binary alloys |
Chemical composition
| Standard | Mg, % | Mn, % | Cu, % | Zn, % | Al, % | OE, % | ET, % |
|---|---|---|---|---|---|---|---|
| DIN 1725 Part 1 | < 0.1 | < 0.1 | < 0.1 | 0.8–1.3 | 98.4–99.2 | < 0.05 | < 0.15 |
Note: Fe + Si < 0.70%
Information on suppliers
Analogues
| Russia | USA |
|---|---|
| АЦпл | 7072 |
Standards
| Standard | Description |
|---|---|
| DIN 1725 Part 1 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| ET | % | Total other items |
| OE | % | Other items |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |