3.5103
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-ferrous metals | Mg Alloys with Th, Zh and Zr |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Cu, % | Zn, % | Ni, % | Zr, % |
|---|---|---|---|---|---|---|---|---|
| DIN 1729 Part 2 | < 0.1 | < 0.1 | 95.615–98.8 | < 0.15 | < 0.03 | 0.8–3 | < 0.005 | 0.4–1 |