Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-ferrous metals | Mg Alloys with Th, Zh and Zr |
Chemical composition
| Standard | Fe, % | Th, % | Si, % | Mg, % | Mn, % | Cu, % | Zn, % | Ni, % | Zr, % |
|---|---|---|---|---|---|---|---|---|---|
| DIN 1729 Part 2 | < 0.01 | 2.7–3.3 | < 0.01 | 92.795–95.2 | < 0.15 | < 0.03 | 1.7–2.7 | < 0.005 | 0.4–1 |